Mechanical Properties Metric English Comments
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Polikim KESTAMID® PA6G Polyamide 6
Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical..
Tensile Modulus 4.00 - 4.80 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
580 - 696 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
depending on color; ISO 527-2/1
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 527-2/1
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6)
Information provided by PolyOne
Tensile Modulus 4.00 GPa
580 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® PP-20GF/000 HS Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Tensile Modulus 4.00 GPa
580 ksi
Plastcom SLOVAMID 6 GF 5 PA6, 5% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 5% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527-1/-2
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data)
Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp..
Tensile Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 450P Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Nilit FRIANYL C73 M-HS3005 Nylon 6.6/6 for injection molding, 30% mineral filled
Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 4.00 GPa
580 ksi
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned)
Key Features:Contains FillerSuitable processing methods:Injection molding
Tensile Modulus 4.00 GPa
580 ksi
1 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif..
Tensile Modulus 4.00 GPa
580 ksi
Conditioned; ISO 527-1,-2
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
Tensile Modulus 4.00 GPa
580 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Tensile Modulus 4.00 GPa
580 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Tensile Modulus 4.00 GPa
580 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Styron CALIBREâ„¢ 7104-8 Polycarbonate
CALIBREâ„¢ 7104-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE..
Tensile Modulus 4.00 GPa
580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL HS2000X PPE+PS
PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E..
Tensile Modulus 4.00 GPa
580 ksi
ASTM-D790
Polyram RamOfin PPH302G4 Polypropylene, 20% Glass Fiber
20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Tensile Modulus 4.00 GPa
580 ksi
Covestro Makrolon® 9415(Z) Polycarbonate
Medium viscosity, flame retardant extrusion and injection molding grade with 10% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia..
Tensile Modulus 4.00 GPa
580 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® BG-15 HM PA6-GF15
Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop..
Tensile Modulus 4.00 GPa
580 ksi
1 mm/min; ISO 527
Eurostar Starglas GX05052 PSU, Glass Fiber Filled
Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar.
Tensile Modulus 4.00 GPa
580 ksi
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber
Contains 10% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 4.00 GPa
580 ksi
ISO 527-1
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade
(PBT+X)-MD40Information provided by BARLOG plastics GmbH.
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Polikim KESTAMID® HS Polyamide 6, Heat Resistant
Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with ..
Tensile Modulus 4.00 GPa
580 ksi
ISO 527-1, 2
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..