Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.903 GPa | 131 ksi | X, Y-Direction; ASTM D638 |
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO.527 DIN.53455 |
Omnia Plastica PE 300 - Polyethylene 300 Molecular weight 300,000 polyethylene similar to the type 500 with higher rigidity and lower resistance to continuous shocks. The applications are similar to those of PE 500, being more commonly spe.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Tensile Modulus | >= 0.900 GPa | >= 131 ksi | 2% sec, MD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4252A (524H1) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer INNOPOL® CS 4-8000 is a polypropylene random copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 4-8000 is highly suitable for pressure pipe manufacturing, includi.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 |
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | DIN 53457 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | |
Kuraray HYBRAR® PH8 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527 |
Styrolution Styrolux BX6400 SBC Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527-2 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Borealis RA130E-2491 Polypropylene Random Copolymer RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527-1/-2 |
Unitika A1030FR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ASTM D638 |
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6 29% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527-2 |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | ISO 527-1/-2 |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20A Z PA12 Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Tensile Modulus | 0.900 GPa @Temperature 23.0 °C |
131 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.900 GPa | 131 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration.. |