Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
Manufacturer | DuPont Performance Polymers |
Trade Name | Zytel® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.870 g/cc | 0.0314 lb/in³ | |
1.02 g/cc | 0.0368 lb/in³ | DAM; ISO 1183 | |
Viscosity | 57470 cP @Shear Rate 5000 1/s, Temperature 280 °C |
57470 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
81230 cP @Shear Rate 5000 1/s, Temperature 245 °C |
81230 cP @Shear Rate 5000 1/s, Temperature 473 °F |
ISO 11403-1 -2 | |
96410 cP @Shear Rate 5000 1/s, Temperature 230 °C |
96410 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 | |
213500 cP @Shear Rate 500 1/s, Temperature 280 °C |
213500 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
370500 cP @Shear Rate 500 1/s, Temperature 245 °C |
370500 cP @Shear Rate 500 1/s, Temperature 473 °F |
ISO 11403-1 -2 | |
465400 cP @Shear Rate 500 1/s, Temperature 230 °C |
465400 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 | |
Viscosity Test | 55 cm³/g | 55 cm³/g | DAM; ISO 307 1157 1628 |
Linear Mold Shrinkage, Flow | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
DAM; ISO 527-1/-2 |
Elongation at Break | >= 50 % | >= 50 % | DAM; ISO 527-1/-2 |
Tensile Modulus | 0.900 GPa | 131 ksi | DAM; ISO 527-1/-2 |
Flexural Modulus | 0.880 GPa | 128 ksi | DAM; ISO 178 |
Izod Impact, Notched (ISO) | NB | NB | DAM; ISO 180/1A |
Charpy Impact, Notched | 13.5 J/cm² | 64.2 ft-lb/in² | DAM; ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.70 J/g-°C | 0.645 BTU/lb-°F | |
Thermal Conductivity | 0.160 W/m-K | 1.11 BTU-in/hr-ft²-°F | of melt |
Melting Point | 221 °C | 430 °F | DAM; 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 0.46 MPa (66 psi) | 55.0 °C | 131 °F | DAM; ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 48.0 °C | 118 °F | DAM; ISO 75-1/-2 |
Glass Transition Temp, Tg | 60.0 °C | 140 °F | DAM; 10°C/min; ISO 11357-1/-2 |
Descriptive Properties | Value | Comments |
---|---|---|
Delivery Form | Pellets | |
Part Marking Code | >PA6-F< | ISO 11469 |
Processing | Blow Moulding | |
Coatable | ||
Film Extrusion | ||
Injection Moulding | ||
Other Extrusion | ||
Profile Extrusion | ||
Sheet Extrusion | ||
Regional Availability | Asia Pacific | |
Europe | ||
Global | ||
Near East/Africa | ||
North America | ||
South and Central America | ||
Resin Identification | PA6-F | |
PA6-F | ISO 1043 | |
Special Characteristics | Heat stabilised or stable to heat |