Solvay TECHNYL® B 230 PA66/6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 230 PA66/6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL ® B 230 is particularly recommended for applications where good impact resistance at low and room temperature is required , also for parts which could break during assembly or parts used at low humidity levels. This grade is commonly used in: automotive industry: bumpers and clips sports and leisure: sports bag buckles and electrical appliance: cable ties. This product is available in natural, black, and in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527 Type 1A
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527 type 1 A
Elongation at Break 250 %
250 %
ISO 527 Type 1A
Tensile Modulus 0.900 GPa
131 ksi
ISO 527 Type 1A
Flexural Strength 27.0 MPa
3920 psi
ISO 178
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Dissipation Factor 0.070
0.070
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %