Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Nilit FRIANYL A63 W-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Nilit FRIANYL B63 KV40 Nylon 6 for injection molding, 40% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK601 BK851 PBT
(Unverified Data**) Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ASTM D638 |
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1,-2 |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance, good surface, good flowability (Easy Flow), low warpage |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
LATI Latilub 62-06GR PA6, Graphite Reinforced Self-lubricating product based on Polyamide 6 (PA6). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 120 °C |
653 ksi @Temperature 248 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East) GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MH0200A PP (Europe-Africa-Middle East) LNP* Thermocomp* MH0200A is a compound based on Polypropylene resin containing High Specific Gravity Filler.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber 15% Glass fiber reinforced polypropylene for injection molding application.Information provided by Polyram. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
DSM Arnite® TV6 220 PBT-GF10 10% Glass Reinforced |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TQ261F2 PA46-GF10 10% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-2A NZ PA12-GF20 Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a .. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey Information provided by Eurotec® |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
BASF Procom® T40H 550 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
BASF Procom® T40H 564 Polypropylene Car heater casings.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
DSM Arnite® TB6 260 PBT-GB30 |