Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.20 GPa | 609 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | Type 1B, 50mm/min; ISO 527-1/2:1993 |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | CD; DIN EN ISO 527 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-2/1A |
Radici Raditer® B RVA 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Tensile Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
Type I, 5.0 mm/min; ISO 527 |
PolyOne Edgetek® QT-20MN/000 natural HI Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY ZF3021 PPE+PS (Europe-Africa-Middle East) LNP* STAT-LOY* ZF3021 is a compound based on PPE + PS Blend resin containing Glass Fiber. Added features include Antistatic, Flame Retardant. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF0029 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WB006 PBT LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp WFB51 PBT LNP THERMOCOMP* WFB51 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Glass Fiber. Added features of this material include: Low Warpage.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM-D790 |
Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled 30% mineral filled, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527-1/-2 |
Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.20 GPa @Temperature 90.0 °C |
610 ksi @Temperature 194 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 1030 GF HI ABS / Nylon 6 Blend, 15% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.15% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ASTM D638 |
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, .. |
|||
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |