Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Mineral Filled |
Manufacturer | CP-Polymer-Technik GmbH & Co. |
Trade Name | Wellamid® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Dry.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 2.0 - 2.5 % | 2.0 - 2.5 % | 23°C/50%RH; DIN 53495 |
Linear Mold Shrinkage | 0.0080 - 0.012 cm/cm @Thickness 4.00 mm |
0.0080 - 0.012 in/in @Thickness 0.157 in |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 75.0 MPa | 10900 psi | 5 mm/min; ISO 527 |
Elongation at Break | 7.0 % | 7.0 % | 5 mm/min; ISO 527 |
Tensile Modulus | 4.20 GPa | 609 ksi | ISO 527 |
Flexural Modulus | 3.60 GPa | 522 ksi | DIN 52457 |
Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
Melting Point | 215 °C | 419 °F | Kofler |
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 179 |
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ISO 179 |
Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Stufe; IEC 707 |
HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
Stufe; IEC 707 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 |
Dielectric Constant | 4.0 @Frequency 1e+6 Hz |
4.0 @Frequency 1e+6 Hz |
IEC 250 |
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
Dielectric Loss Index | 0.020 | 0.020 | At 1 MHz; IEC 250 |
Comparative Tracking Index | 450 V | 450 V | Stufe; IEC 112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 - 290 °C | 500 - 554 °F | |
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Back Pressure | Low | |
Holding Pressure | High | |
Injection Speed | High | |
Screw Speed | High |