Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.00 GPa | 580 ksi | ISO.527 DIN.53455 |
Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ASTM D638 |
NCMT NanoPAC™ G2000 High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Nilit FRIANYL B63 KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 G 10 Polyamide 6, 10% Graphite FeaturesPA 6 for injection moulding with addition of 10% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, sli.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® APTIV® 2102-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
(discontinued ** APTIV PEEK 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Nilit RECONYL B KV30 Recycled nylon 6 for injection molding, 30% glass ball reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 7616 000000 PBT + PC, 15% Glass Fiber PBT+PC, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | Conditioned; ISO 527-1,-2 |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
LATI Latiohm 88/10-06 CNT PEEK Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Styron CALIBREâ„¢ 7104-8 Polycarbonate CALIBREâ„¢ 7104-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ASTM D4894 |
Saint-Gobain Fluoroloy® A22 High Performance Seal Material High modulus with excellent high-temperature resistance; Abrasion resistant; Chemically Inert; Recommended for back-up rings and for special applications.
Information provided by Saint-Gobain P.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage toleran.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1 mm/min; ISO 527 |
Eurostar Starglas GX05052 PSU, Glass Fiber Filled Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecomid® NT40 NL XA60 PPA, unfilled, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002 Information provided by Eurotec® |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
BASF Gusspolyamid® Nylon 6 (Dry As Molded) Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | 1mm/min; ISO 527 |
Teijin Panlite® GS-3410 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527 |
Polikim KESTAMID® HS Polyamide 6, Heat Resistant Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with .. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, Conditioned Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Tensile Modulus | 4.00 GPa | 580 ksi | |
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |