Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexPly® M42 is a high performance, self extinguishing, self adhesive, tough epoxy matrix for use in primary aerospace sandwich structures. It exhibits very high impact resistance and damage tolerance for a wide range of applications. HexPly® M42 is a toughened epoxy resin system supplied with woven glass, carbon and hybrid glass/carbon fibers. HexPly® M42 was developed as a controlled flow system to operate in environments up to 120-130°C.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 77.0 MPa
11200 psi
Elongation at Yield 1.59 %
1.59 %
Tensile Modulus 4.00 GPa
580 ksi
Poissons Ratio 0.40
0.40
Fracture Toughness 1.83 MPa-m½
1.67 ksi-in½
Shear Modulus 1.43 GPa
207 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 59.1 µm/m-°C
32.8 µin/in-°F
Maximum Service Temperature, Air 120 - 130 °C
248 - 266 °F
Glass Transition Temp, Tg 153 °C
307 °F
Wet, 14 days in water @ 70°C.
193 °C
379 °F
Dry
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F