Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Omnia Plastica s.p.a.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitable for gears and mechanical parts where excellent wear resistance is required.Features:Very high wear resistance: this inherent polyamide feature is further increased by the addition of glass. Akulon GF is one of the best wear resistant plastic materials available.High compression strength and tensile stress: the fatigue resistance is excellent as are the general mechanical properties.Ageing resistance: weatherproof and good resistance at low temperatureBlack colour.Weak Point:If used in combination with moving parts, the glass filler causes abrasion of the steel parts in contact with the plastic.Application:Mechanical: very high compressive strength and wear resistance, in fact one the best of all the engineering plastics. This material is particularly suitable for gears and high performance mechanical components which need to operate in demanding environments, such as on construction equipment or earthmovers, without suffering from excessive wear.Food contact: it cannot be used in contact with food.Electrical: even though the electrical properties change with the moisture content, this nylon is still used where good mechanical features as well as weatherproof performance are required.Chemical: it is resistant to alkali, inorganic compounds and solvents.Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% relative humidity (beginning dry)
Water Absorption at Saturation 5.2 %
5.2 %
23°C (beginning dry)
Mechanical Properties Metric English Comments
Ball Indentation Hardness 170 MPa
24700 psi
ISO2039.1 DIN.53456
Tensile Strength at Break 100 MPa
14500 psi
ISO.527 DIN.53455
Elongation at Break 20 %
20 %
ISO.527 DIN.53455
Tensile Modulus 4.00 GPa
580 ksi
ISO.527 DIN.53455
Compressive Strength 15.0 MPa
2180 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NB
NB
7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.50
0.50
on dry ground steel; load =0.05MPa; speed =0.6 m/s (dry sample)
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F

@Temperature 73.4 - 140 °F
dry sample
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN.52612 (dry sample)
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 105 °C
221 °F
Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample)
170 °C
338 °F
short period, no load (dry sample)
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ISO.75 DIN.53461 (dry sample)
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
impact conditions and heavy loads not considered (dry sample)
Electrical Properties Metric English Comments
Dielectric Constant 7.0

@Frequency 1e+6 Hz
7.0

@Frequency 1e+6 Hz
ISO.250 DIN.53483
Copyright © lookpolymers.com All Rights Reserved