Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NCMT NanoPAC™ G2000 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF NCMT NanoPAC™ G2000 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
NCMT Method
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 4.00 GPa
580 ksi
ASTM D638
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection Temp.; ASTM D648