Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.17 GPa | 315 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM Data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM D638 |
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.17 GPa @Thickness 3.20 mm |
314 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM-D638 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific) LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM D638 |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM D638 |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM D638 |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | Storage |
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-PFC is a two component, semiconductor grade epoxy, designed for flip chip interconnects using a solder-free joining method.Advantages & Application Notes: Stencil.. |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | ASTM D638 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Tensile Modulus | 2.17 GPa | 315 ksi | 1 mm/min |
Arkema Group Appryl® CWE 1020 Polypropylene, 20% Talc Filled Compound of a PP copolymer and 20% aesthetic talc. This grade has been specially developed for interior trim automotive applications, that required an excellent scratch resistance associated with a .. |