Material Notes:
LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 6.6 %
6.6 %
ASTM D638
Tensile Modulus 2.17 GPa
315 ksi
50 mm/min; ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.84 J/cm
7.19 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C

@Thickness 3.20 mm
163 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257