Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D 792
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.10 %
0.10 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.10 %

@Temperature 23.0 °C
0.10 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
8.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
10 g/10 min

@Load 5.00 kg,
Temperature 265 °C
10 g/10 min

@Load 11.0 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527
56.0 MPa
8120 psi
Type I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ISO 527
57.0 MPa
8270 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ISO 527
125 %
125 %
Type I, 50 mm/min; ASTM D 638
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527
4.9 %
4.9 %
Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2.17 GPa
315 ksi
5 mm/min; ASTM D 638
2.25 GPa
326 ksi
1 mm/min; ISO 527
Flexural Yield Strength 85.0 MPa
12300 psi
1.3 mm/min, 50 mm span; ASTM D 790
85.0 MPa
12300 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 5.30 J/cm

@Temperature -30.0 °C
9.93 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 35.0 kJ/m²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
50.0 kJ/m²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
72.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 124 °C

@Thickness 3.20 mm
255 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
107 °C

@Thickness 3.20 mm
225 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 118 °C
244 °F
Rate B/50; ASTM D 1525
118 °C
244 °F
Rate B/50; ISO 306
122 °C
252 °F
Rate B/120; ISO 306
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2