Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Tensile Strength, Yield | 48.3 - 58.6 MPa | 7000 - 8500 psi | ASTM D638 |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources AC-G25 Acetal Copolymer, 25% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
(discontinued **) Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-10GB/000 Black Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Electrablend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF30 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good UV ResistanceAdditive: UV StabilizerInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® POM CO 0241 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D-882 |
Saint-Gobain Norton® ETFE Fluoropolymer Film Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa @Thickness 3.17 mm |
7000 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Westlake Plastics Kynar® 1000HD PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D-638 |
Axiall 3014 Rigid PVC, Extrusion Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Luriblend® POM HO TL20 BK Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D-638 |
Axiall 5009 Rigid PVC, Molding Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D-638 |
Axiall 6511 Rigid PVC, Molding Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformab.. |
|||
Tensile Strength, Yield | >= 48.3 MPa | >= 7000 psi | ASTM D638 |
Buckeye Polymers BP RPP 3009 GK BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-10GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |