Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
Reliance Industries Polypropylene - 40% Suzorex mica (surface treated) filled Information provided by Reliance Industries |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
Rotuba H5 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO R527 |
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC (Asia Pacific) Impact modified, highly chemical resistant polyester/polycarbonate alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PH1100B PA 6 LNP* THERMOCOMP* PH1100B is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50mm/min; ISO 527-2 |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | parallel; ISO 527-3 |
Covestro Desmopan® W DP89056D Polyurethane PreprocessingMax. Water content |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
Fainplast Compounds R 220/R Rigid PVC, Extrusion Shiny rolling shutters |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO R527 |
Fainplast Compounds ART 0699 Rigid PVC, Atoxic for General Purpose Bottles suitable for containing oils |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO R527 |
Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose Transparent bottles medium/high antishock |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50mm/min; ISO 527 |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527-2 |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Tensile Strength, Yield | 43.0 - 53.1 MPa | 6240 - 7700 psi | Average value: 47.9 MPa Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |