| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D 792 |
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.50 % @Temperature 23.0 °C |
0.50 % @Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | on tensile bar; SABIC Method |
| 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.1 g/10 min @Load 5.00 kg, Temperature 260 °C |
7.1 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
| 7.2 g/10 min @Load 3.80 kg, Temperature 280 °C |
7.2 g/10 min @Load 8.38 lb, Temperature 536 °F |
ASTM D 1238 | |
| 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 | |
| 9.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 100 | 100 | ASTM D 785 |
| Tensile Strength at Break | 36.0 MPa | 5220 psi | Type I, 5 mm/min; ASTM D 638 |
| 36.0 MPa | 5220 psi | 50 mm/min; ISO 527 | |
| 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D 638 | |
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D 638 |
| 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 | |
| 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D 638 | |
| Elongation at Break | 26 % | 26 % | Type I, 50 mm/min; ASTM D 638 |
| 27 % | 27 % | Type I, 5 mm/min; ASTM D 638 | |
| 36 % | 36 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D 638 |
| 2.7 % | 2.7 % | Type I, 50 mm/min; ASTM D 638 | |
| 2.8 % | 2.8 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
| 2.36 GPa | 342 ksi | 5 mm/min; ASTM D 638 | |
| 2.40 GPa | 348 ksi | 50 mm/min; ASTM D 638 | |
| Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
| 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Flexural Modulus | 2.38 GPa | 345 ksi | 2 mm/min; ISO 178 |
| 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 | |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| 36.0 J @Temperature 23.0 °C |
26.6 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 84.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 94.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 94.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 97.0 °C @Thickness 3.20 mm |
207 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 95.0 °C | 203 °F | Rate B/50; ISO 306 |
| 98.0 °C | 208 °F | Rate B/50; ASTM D 1525 | |
| 99.0 °C | 210 °F | Rate B/120; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 93 % | 93 % | untextured, 60 degrees; ASTM D 523 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | Pass85 | IEC 60695-10-2 |
| UV-light, water exposure/immersion | F1 | UL 746C |