Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Transparent bottles medium/high antishock
Physical Properties Metric English Comments
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 43.0 MPa
6240 psi
ISO R 527
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO R527
Elongation at Break 140 %
140 %
ISO R 527
Izod Impact, Unnotched 5.80 - 6.20 J/cm

@Temperature 23.0 °C
10.9 - 11.6 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 75.0 - 77.0 °C

@Load 5.00 kg
167 - 171 °F

@Load 11.0 lb
ISO R306
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified