| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP Stat-loy |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-LOY AF306 ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
| 1.29 g/cc | 0.0466 lb/in³ | ASTM D792 | |
| Moisture Absorption | 3.00 % | 3.00 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm <br>@Time 86400 sec |
0.0020 - 0.0040 in/in <br>@Time 24.0 hour |
ASTM D955 |
| 0.0030 cm/cm <br>@Time 86400 sec |
0.0030 in/in <br>@Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0045 cm/cm <br>@Time 86400 sec |
0.0045 in/in <br>@Time 24.0 hour |
ISO 294 |
| 0.0040 - 0.0060 cm/cm <br>@Time 86400 sec |
0.0040 - 0.0060 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 38.0 MPa | 5510 psi | ASTM D638 |
| 43.0 MPa | 6240 psi | ISO 527 | |
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
| 43.0 MPa | 6240 psi | ISO 527 | |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| 1.0 % | 1.0 % | ISO 527 | |
| Elongation at Yield | 1.0 % | 1.0 % | ASTM D638 |
| 1.1 % | 1.1 % | ISO 527 | |
| Tensile Modulus | 6.01 GPa | 872 ksi | 1 mm/min; ISO 527 |
| 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 48.0 MPa | 6960 psi | ASTM D790 |
| 63.0 MPa | 9140 psi | ISO 178 | |
| Flexural Modulus | 5.51 GPa | 799 ksi | ASTM D790 |
| 5.70 GPa | 827 ksi | ISO 178 | |
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 2.50 J/cm | 4.68 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 113 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 114 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 43.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
23.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 43.2 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 102 °C <br>@Thickness 3.20 mm |
216 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 71.0 °C | 160 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 95.0 °C <br>@Thickness 3.20 mm |
203 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |