Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Transparent antishock profiles
Physical Properties Metric English Comments
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO R 527
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO R527
Elongation at Break 140 %
140 %
ISO R 527
Izod Impact, Unnotched 0.800 - 1.20 J/cm

@Temperature 23.0 °C
1.50 - 2.25 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 63.0 - 65.0 °C

@Load 5.00 kg
145 - 149 °F

@Load 11.0 lb
ISO R306
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Users viewing this material also viewed the following: