Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Izod Impact, Notched (ISO) | 6.50 - 10.0 kJ/m² | 3.09 - 4.76 ft-lb/in² | Average value: 8.09 kJ/m² Grade Count:4 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) EPV 31 RA Polypropylene A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced 20% Mineral Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 9220 is a nucleated random copolymer polypropylene with a melt flow index of 20 g/10 min for the injection molding of articles with high transparency and excellent surface a.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ASTM D256 |
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ASTM D256 |
Total PSI 2451 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Polyram RamTough PZ303G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 XEC1 POM Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe .. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 211 V20 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 ZM30 Nylon 6, 30% Mineral Filled Mineral filled, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Izod Impact, Notched (ISO) | 6.50 - 16.0 kJ/m² | 3.09 - 7.61 ft-lb/in² | Average value: 11.0 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |