Material Notes:
Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applications for Total Petrochemicals Polystyrene 850S include TV covers, Decoders, Hi-Fi and Internal parts for office equipment.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Spiral Flow 35.0 cm

@Temperature 220 °C
13.8 in

@Temperature 428 °F
ASTM D3123
52.0 cm

@Temperature 260 °C
20.5 in

@Temperature 500 °F
ASTM D3123
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength at Break 36.0 MPa
5220 psi
ASTM D638
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
ASTM D696
Vicat Softening Point 96.0 °C

@Load 1.02 kg
205 °F

@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature >= 82.2 °C
>= 180 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC 93
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149