Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® ECO PA GF30 909040 Nylon 6, 30% Glass Fiber PA 6 (mainly), 30% glass fibers, injection molding, contains at least 80% pre-consumer recycled material, properties may change considerably from lot to lotInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DX07035 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DX07035 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame retardant, Easy Molding, Internally Lubricated, Mold R.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP HAL23 PA11 (Europe-Africa-Middle East) LNP* LUBRICOMP* HAL23 is a compound based on PA 11 resin containing Aramid Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 48.0 kJ/m² | 19.0 - 22.8 ft-lb/in² | Type 1; ISO 180 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East) Color Stable Glass filled PET |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF006ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp PX05046 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PX05046 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europ.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF005Z PA66, 25% Glass Fiber, Injection Molded Starflam RF005Z is a 25% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide RF1005E-BK82205)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starglas GX05052 PSU, Glass Fiber Filled Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | DIN 53453 |
Ineos Nova S-3201 Medium Impact Compact Polystyrene
(discontinued **) Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to .. |
|||
Izod Impact, Unnotched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 68.0 kJ/m² | 19.0 - 32.4 ft-lb/in² | Average value: 50.7 kJ/m² Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |