Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Europe-Africa-Middle East) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
15.7 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 44.3 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 - 80.0 kJ/m² | 15.7 - 38.1 ft-lb/in² | Average value: 52.0 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL8008T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific) LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF005 PA 66 LNP* THERMOCOMP* RF005 is a compound based on Nylon 66 resin containing 25% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |