Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® INP222 ABS Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | |
Reliance Industries Polypropylene - Virgin Polypropylene Information provided by Reliance Industries |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ HPP TF20 V0 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature -30.0 °C |
0.450 ft-lb/in @Temperature -22.0 °F |
ASTM D256A |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Izod Impact, Notched | 0.240 - 7.74 J/cm | 0.450 - 14.5 ft-lb/in | Average value: 0.842 J/cm Grade Count:66 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Notched | 0.240 - 0.290 J/cm | 0.450 - 0.543 ft-lb/in | Average value: 0.259 J/cm Grade Count:15 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature 23.0 °C |
0.450 ft-lb/in @Temperature 73.4 °F |
1/8'' notched bar; ASTM D256 |
Ineos H53N-00 Polypropylene Homopolymer This is a high flow rate nucleated and lightly lubricated homopolymer polypropylene designed for high-speed injection molding of thin-walled parts requiring good stiffness and fast cycle times. Thi.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature 22.8 °C |
0.450 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene CPP1050 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Izod Impact, Notched | >= 0.240 J/cm | >= 0.450 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Izod Impact, Notched | >= 0.240 J/cm | >= 0.450 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Izod Impact, Notched | 0.240 - 0.260 J/cm | 0.450 - 0.487 ft-lb/in | ASTM D256A |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Bapolene® 4071 Polypropylene, Fiber/Injection Grade Bapolene PP4071 is a high flow PP homopolymer for staple and continuous filament applications as well as general purpose injection molding. This resin exhibits good melt and thermal stability.Appli.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | |
Abatron AboCast 50-11/AboCure 50-17 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/27 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 270°C (520°F). Cures in 1-2 hrs at .. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P-40TC-0158 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.240 J/cm @Temperature -40.0 °C |
0.450 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® L925 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. The natural c.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Perstorp Compounds Akestra™ 110 Thermoplastic Copolyester Transparent sparkling glass-like appearance. Suitable for films, sheets, blow molding, foams and injection molding. It can be used as a polystyrene alternative for heat resistant thin wall contain.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
Izod Impact, Notched | 0.240 J/cm | 0.450 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group |