Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm |
2.20 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO Uses include electric/electronic parts. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN163G30 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
Kolon Kopa® KN163G30 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® N601G30 Nylon 66, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9120AT ASA, Unreinforced Used in washing machine cover etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9120AT ASA, Unreinforced Used in washing machine cover etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX4716 PPE+HIPS (Asia Pacific) PPE+PS GF15% FR V-1 |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | |
Zylog Hipolyene® 9221 XM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML3430 PC, 30% Glass Fiber |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® J910 10% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G701H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | Wet; ASTM D256 |
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G701V Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 1.18 J/cm | 2.20 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G6-33GF Nylon 66, 33% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.18 J/cm @Thickness 3.17 mm |
2.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® SD6350T PMMA, Opaque High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |