Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Thickness 3.20 mm
0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 43.1 MPa
6260 psi
5 mm/min; ASTM D638
Elongation at Break 15 %
15 %
5 mm/min; ASTM D638
Flexural Strength 60.8 MPa
8820 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.18 J/cm

@Thickness 6.35 mm
2.20 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.40 mm
212 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 113 °C
235 °F
B/50; ISO R306