Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, GOOD FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING, INJECTION STRETCH BLOW MOLDING (ISBM) FOR FOOD CONTAINERS, BOTTLES, HOUSEWARES, CRATES |
|||
Izod Impact, Notched | >= 0.420 J/cm | >= 0.787 ft-lb/in | Method A; ASTM D 256 |
Karina E 835-10/156-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 4521 PBT VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 LNP THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing 15% Glass Fiber. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf VFM53 PA 66 (Asia Pacific) LNP* THERMOTUF* VFM53 is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX03633C PC LNP STAT-KON* DX03633C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256A |
Total PPH 3281 Polypropylene, Extrusion Grade Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.787 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |