Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
Polycasa Acryl® G 66 Acrylic, Injection Molding Grade Injection molding grade used for: Fresnel lenses, filter screens for TVs and VDUs, drawing instruments.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as .. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Charpy Impact, Notched | 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² @Temperature 23.0 °C |
0.952 - 1.43 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Charpy Impact, Notched | 0.200 - 0.600 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 2.86 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.450 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact, Notched | 0.200 - 0.400 J/cm² @Temperature 23.0 °C |
0.952 - 1.90 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Charpy Impact, Notched | 0.200 - 7.50 J/cm² | 0.952 - 35.7 ft-lb/in² | Average value: 1.07 J/cm² Grade Count:127 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
LATI Latistat 52/7-02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179 |
Styrolution Styrolux S SBC Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film appli.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ASTM D256 |
Plenco 4548 Phenolic, Granular, Transfer Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | ISO 179 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO Data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 30.0 °C |
0.952 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179-2 |
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Charpy Impact, Notched | 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TB6 260 PBT-GB30 |
|||
Charpy Impact, Notched | 0.200 - 2.60 J/cm² @Temperature -20.0 - -20.0 °C |
0.952 - 12.4 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.39 J/cm² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.200 - 2.60 J/cm² @Thickness 102 - 102 mm |
0.952 - 12.4 ft-lb/in² @Thickness 4.00 - 4.00 in |
Average value: 1.39 J/cm² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |