Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 - 0.600 J/cm²

@Temperature 23.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
Charpy Impact, Notched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Injection and Compression; ISO 179/1eA
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel..
Charpy Impact, Notched 0.400 - 0.600 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.529 J/cm² Grade Count:6
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Charpy Impact, Notched 0.200 - 0.600 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 2.86 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.450 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Charpy Impact, Notched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Charpy Impact, Notched 0.550 - 0.600 J/cm²

@Temperature -20.0 - -20.0 °C
2.62 - 2.86 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.590 J/cm² Grade Count:5
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Charpy Impact, Notched 0.0300 - 0.600 J/cm²

@Temperature -30.0 - -20.0 °C
0.143 - 2.86 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.289 J/cm² Grade Count:43
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Charpy Impact, Notched 0.280 - 0.600 J/cm²
1.33 - 2.86 ft-lb/in²
Average value: 0.398 J/cm² Grade Count:6
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 0.450 - 0.600 J/cm²
2.14 - 2.86 ft-lb/in²
Average value: 0.550 J/cm² Grade Count:3
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Charpy Impact, Notched 0.500 - 0.600 J/cm²

@Temperature -20.0 - -20.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.550 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Charpy Impact, Notched 0.600 - 0.600 J/cm²

@Temperature -20.0 - -20.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.600 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Charpy Impact, Notched 0.300 - 0.600 J/cm²
1.43 - 2.86 ft-lb/in²
Average value: 0.467 J/cm² Grade Count:6
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.100 - 0.600 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.193 J/cm² Grade Count:46
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Charpy Impact, Notched 0.530 - 0.600 J/cm²

@Temperature -40.0 - -30.0 °C
2.52 - 2.86 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.560 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Copyright © lookpolymers.com All Rights Reserved