Polymer Property : Charpy Impact, Notched = 0.952 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Polycasa Acryl® G 66 Acrylic, Injection Molding Grade
Injection molding grade used for: Fresnel lenses, filter screens for TVs and VDUs, drawing instruments.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as ..
Charpy Impact, Notched 0.200 - 0.300 J/cm²
0.952 - 1.43 ft-lb/in²
Injection; ISO 179/ 1eA
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Charpy Impact, Notched 0.200 - 0.400 J/cm²
0.952 - 1.90 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Charpy Impact, Notched 0.200 - 0.300 J/cm²

@Temperature 23.0 °C
0.952 - 1.43 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Polycasa Acryl® G 88 E Acrylic
Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs ..
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.396 J/cm² Grade Count:23
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO Data, Low Temp
Americas Styrenics Styron® 6010 High Impact Polystyrene  (discontinued **)
STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac..
Charpy Impact, Notched 0.200 - 0.400 J/cm²

@Temperature 23.0 °C
0.952 - 1.90 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Charpy Impact, Notched 0.200 - 0.700 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.445 J/cm² Grade Count:20
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ASTM D256
Plenco 7466 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406..
Charpy Impact, Notched 0.200 - 2.50 J/cm²

@Temperature -30.0 - 30.0 °C
0.952 - 11.9 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.832 J/cm² Grade Count:29
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Charpy Impact, Notched 0.200 - 1.50 J/cm²
0.952 - 7.14 ft-lb/in²
Average value: 0.533 J/cm² Grade Count:11
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® CMG302 Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
LATI Laticonther 52/11 GR/70 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 0.000 °C
0.952 ft-lb/in²

@Temperature 32.0 °F
80*10*4mm, Cut; ISO 179/1eA
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP
SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.
Charpy Impact, Notched 0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179-1
Unitika CX-2500 PA6, Conditioned
Transparent nylonInformation provided by Unitika Ltd.
Charpy Impact, Notched 0.200 J/cm²

@Temperature 30.0 °C
0.952 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR
Information provided by EMS Grivory
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO Data, Low Temp
Dow AIM® 4800 High Impact Styrenic Resin
AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade
Injection moldingsData was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3520 L Polypropylene
Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 300 MW4 POM
Mineral filled injection molding grade based on Tarnoform 300 reinforced with 20% wollastonite; such a compound has high stiffness, dimensional stability and hardness combined with low shrinkage.Inf..
Charpy Impact, Notched 0.200 - 0.500 J/cm²

@Temperature -20.0 - 30.0 °C
0.952 - 2.38 ft-lb/in²

@Temperature -4.00 - 86.0 °F
Average value: 0.350 J/cm² Grade Count:5
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 30.0 °C
0.952 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® G 21 PA6I/6T
Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle..
Charpy Impact, Notched 0.200 - 0.500 J/cm²

@Temperature -20.0 - -20.0 °C
0.952 - 2.38 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.340 J/cm² Grade Count:5
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.200 - 2.70 J/cm²
0.952 - 12.8 ft-lb/in²
Average value: 1.11 J/cm² Grade Count:55
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..