Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 - 0.350 J/cm² | 0.714 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact, Notched | 0.150 - 0.350 J/cm² | 0.714 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179/1eA |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Charpy Impact, Notched | 0.150 J/cm² - NB @Temperature -40.0 - -20.0 °C |
0.714 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 0.311 J/cm² Grade Count:15 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² @Temperature -40.0 - 30.0 °C |
0.714 - 3.81 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.357 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Latigray 62-01 CX/75 PA 6 Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade Injection moldingsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 13.0 J/cm² | 0.714 - 61.9 ft-lb/in² | Average value: 1.44 J/cm² Grade Count:56 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.278 J/cm² Grade Count:9 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 VC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 UC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 9.00 J/cm² | 0.714 - 42.8 ft-lb/in² | Average value: 0.657 J/cm² Grade Count:53 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² | 0.714 - 3.81 ft-lb/in² | Average value: 0.405 J/cm² Grade Count:11 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.317 J/cm² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.150 J/cm² - NB @Temperature -40.0 - -20.0 °C |
0.714 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 0.997 J/cm² Grade Count:99 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |