| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded |
| Manufacturer | BASF |
| Trade Name | Novolen® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Novolen® 3300 MC Polypropylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.910 g/cc | 0.0329 lb/in³ | |
| Water Absorption | 0.10 % | 0.10 % | |
| Moisture Absorption at Equilibrium | 0.10 % | 0.10 % | |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
| Melt Flow | 11 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
11 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
| Elongation at Break | >= 50 % | >= 50 % | |
| Elongation at Yield | 12 % | 12 % | |
| Tensile Modulus | 0.700 GPa | 102 ksi | |
| Charpy Impact Unnotched | NB | NB | |
| 1.80 J/cm² <br>@Temperature -30.0 °C |
8.57 ft-lb/in² <br>@Temperature -22.0 °F |
||
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
| 0.150 J/cm² <br>@Temperature -30.0 °C |
0.714 ft-lb/in² <br>@Temperature -22.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 185 µm/m-°C <br>@Temperature 20.0 °C |
103 µin/in-°F <br>@Temperature 68.0 °F |
|
| Melting Point | 139 °C | 282 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 59.0 °C | 138 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 44.0 °C | 111 °F | |
| Vicat Softening Point | 53.0 °C | 127 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
| Dielectric Constant | 2.3 <br>@Frequency 1e+6 Hz |
2.3 <br>@Frequency 1e+6 Hz |
|
| Dielectric Strength | 140 kV/mm | 3560 kV/in | |
| Dissipation Factor | 0.000070 <br>@Frequency 100 Hz |
0.000070 <br>@Frequency 100 Hz |
|
| 0.00020 <br>@Frequency 1e+6 Hz |
0.00020 <br>@Frequency 1e+6 Hz |
||
| Comparative Tracking Index | 600 V | 600 V |