| Category | Polymer , Thermoset , Phenolic |
| Manufacturer | Raschig Group |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Raschig Group DECAL® 5431 Phenolic.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 - 1.45 g/cc | 1.35 - 1.45 g/cc | ISO 1183 |
| Apparent Bulk Density | 0.550 - 0.700 g/cc | 0.0199 - 0.0253 lb/in³ | ISO 60 |
| Water Absorption | <= 1.50 % <br>@Temperature 23.0 °C,<br> Time 86400 sec |
<= 1.50 % <br>@Temperature 73.4 °F,<br> Time 24.0 hour |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.00600 - 0.00800 cm/cm | 0.00600 - 0.00800 in/in | Injection and Compression; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection and Compression; ISO 527 |
| Modulus of Elasticity | 3.00 - 5.00 GPa | 435 - 725 ksi | Compression; ISO 527 |
| 4.00 - 6.00 GPa | 580 - 870 ksi | Injection; ISO 527 | |
| Flexural Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 178 |
| 90.0 - 110 MPa | 13100 - 16000 psi | Injection; ISO 178 | |
| Flexural Modulus | 6.00 - 8.00 GPa | 870 - 1160 ksi | Injection and Compression; ISO 178 |
| Compressive Strength | 200 - 250 MPa | 29000 - 36300 psi | ISO 604 |
| Charpy Impact Unnotched | 0.400 - 0.600 J/cm² | 1.90 - 2.86 ft-lb/in² | Compression; ISO 179/1eU |
| 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU | |
| Charpy Impact, Notched | 0.150 - 0.350 J/cm² | 0.714 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
| 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Injection; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 - 35.0 µm/m-°C <br>@Temperature 50.0 - 150 °C |
13.9 - 19.4 µin/in-°F <br>@Temperature 122 - 302 °F |
ISO 11359-2 |
| Thermal Conductivity | 0.200 - 0.400 W/m-K | 1.39 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461 |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 - 180 °C | 320 - 356 °F | ISO 75-A |
| Deflection Temperature at 8.0 MPa | 100 - 120 °C | 212 - 248 °F | ISO 75-C |
| Flammability, UL94 | V-0 <br>@Thickness 3.60 mm |
V-0 <br>@Thickness 0.142 in |
|
| Shrinkage | 0.400 - 0.600 % <br>@Temperature 110 °C,<br> Time 605000 sec |
0.400 - 0.600 % <br>@Temperature 230 °F,<br> Time 168 hour |
Post shrinkage; ISO 2577 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 - 1.00e+17 ohm-cm | 1.00e+16 - 1.00e+17 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | IEC 60093 |
| Dielectric Constant | 4.00 - 6.00 <br>@Frequency 1.00e+6 Hz |
4.00 - 6.00 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 12.0 - 16.0 <br>@Frequency 100 Hz |
12.0 - 16.0 <br>@Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 20.0 - 30.0 kV/mm | 508 - 762 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0600 - 0.0800 <br>@Frequency 1.00e+6 Hz |
0.0600 - 0.0800 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 0.600 - 0.800 <br>@Frequency 100 Hz |
0.600 - 0.800 <br>@Frequency 100 Hz |
IEC 60250 | |
| Arc Resistance | 60.0 - 120 sec | 60.0 - 120 sec | ASTM D495 |
| Comparative Tracking Index | >= 175 V | >= 175 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 6.00 Month <br>@Temperature 15.0 - 25.0 °C |
6.00 Month <br>@Temperature 59.0 - 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Glow wire flammability test | 900/1 | IEC 60695 2-12 |
| Glow wire ignitability test | 900/1 | IEC 60695 2-13 |
| Water Absorption | <80 mg | 24 hr, 23°C; ISO 62 |