| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183-1 |
| Moisture Absorption at Equilibrium | 1.3 % | 1.3 % | 50% RH |
| Water Absorption at Saturation | 3.0 % | 3.0 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell E | 84 | 84 | ISO 2039-2 |
| Hardness, Shore D | 86 | 86 | |
| Ball Indentation Hardness | 225 MPa | 32600 psi | ISO 2039-1 |
| Tensile Strength | 67.0 MPa | 9720 psi | at Break (NYP); ISO 527-1/-2 |
| Elongation at Break | 2.0 % | 2.0 % | ISO 527-1/-2 |
| Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1/-2 |
| Flexural Strength | 100 MPa | 14500 psi | |
| Compressive Strength | 44.0 MPa @Strain 1 % |
6380 psi @Strain 1 % |
ISO 604 |
| 81.0 MPa @Strain 2 % |
11700 psi @Strain 2 % |
ISO 604 | |
| 145 MPa @Strain 5 % |
21000 psi @Strain 5 % |
ISO 604 | |
| K Factor (ISO) | 55 µm/km | 55 µm/km | |
| Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179-1/1eU |
| Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | ISO 179-1/1eA |
| Coefficient of Friction, Dynamic | 0.25 - 0.40 | 0.25 - 0.40 | |
| Limiting Pressure Velocity | 0.440 MPa-m/sec | 12600 psi-ft/min | at 1 m/s unlubricated |
| 1.20 MPa-m/sec | 34300 psi-ft/min | at 0.1 m/s unlubricated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 36.0 µm/m-°C @Temperature 23.0 - 100 °C |
20.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
| Thermal Conductivity | 0.390 W/m-K | 2.71 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 240 °C | 464 °F | Continuous |
| Deflection Temperature at 1.8 MPa (264 psi) | 365 °C | 689 °F | ISO 75-1/-2 |
| Glass Transition Temp, Tg | 365 °C | 689 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 47 % | 47 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | <= 10000 ohm | <= 10000 ohm | IEC 60093 |
| Dielectric Strength | 13.0 kV/mm | 330 kV/in |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| European Food 1935/2004 | No | No | |
| FDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | Yes | Yes | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |