Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH-SG-GV 2020 Nylon 6.6 for injection molding, 20% mineral filled, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CMH454 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSM-30/2 PA666-MD30 Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell.. |
|||
Ball Indentation Hardness | 190 MPa @Time 30.0 sec |
27600 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Ball Indentation Hardness | 190 MPa @Time 30.0 sec |
27600 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PPS High hardness and stiffness, good abrasion resistance, low moisture absorption, favorable insulating features, low dielectric, high non-inflammability and high chemical resistance are the essential .. |
|||
Ball Indentation Hardness | 190 MPa @Load 98.0 kg, Time 30.0 sec |
27600 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO2039 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Ball Indentation Hardness | 190 MPa @Load 36.5 kg |
27600 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced 25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Ball Indentation Hardness | 190 MPa @Load 98.0 kg, Time 30.0 sec |
27600 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TS V0 X PA666 FR Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Ball Indentation Hardness | 190 MPa | 27600 psi | ISO 2039-1 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Ball Indentation Hardness | 190 MPa @Load 36.5 kg, Time 30.0 sec |
27600 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Ball Indentation Hardness | 190 MPa @Load 98.0 kg, Time 30.0 sec |
27600 psi @Load 216 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |