Material Notes:
Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main properties:Flame retardant system free of halogen compounds and elementary phosphorusUL 94 V-0 down to 0.8 mm thicknessHigh toughnessGood mechanical propertiesRoHS: Grilon XE 5030 complies with the regulations acc. RoHS (2002/95/EC, Restriction of Hazardous Substances).WEEE: Parts made of Grilon XE 5030 are not affected by the demands for “selective recycling” acc. Guideline 2002/96/EC for Electro and Electronic Appliance. Grilon XE 5030 was developed for manufacturing of parts in the field of electric and electronic equipment such as fuses, strips, cable binders, plug-in terminal strips, and coil former bobbins.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
190 MPa
27600 psi
dry; ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
75.0 MPa
10900 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
dry; ISO 527-1/-2
80.0 MPa
11600 psi
dry; ISO 527-1/-2
Elongation at Break 9.0 %
9.0 %
dry; ISO 527-1/-2
9.0 %
9.0 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
25 %
25 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
3.80 GPa
551 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.900 J/cm²
4.28 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.350 J/cm²

@Temperature 30.0 °C
1.67 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Comparative Tracking Index 575 V
575 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Burning Behaviour VDE
Electricals & Electronics Cables & Tubes
Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Form Granules
Processing Injection Molding
Product Attributes Improved flowability and demoulding