Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 90.0 - 230 MPa | 13100 - 33400 psi | Average value: 192 MPa Grade Count:8 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Ball Indentation Hardness | 90.0 - 270 MPa | 13100 - 39200 psi | Average value: 191 MPa Grade Count:5 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Ball Indentation Hardness | 90.0 - 170 MPa | 13100 - 24700 psi | Average value: 121 MPa Grade Count:7 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Ball Indentation Hardness | 90.0 - 225 MPa | 13100 - 32600 psi | Average value: 173 MPa Grade Count:16 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039 |
GEHR Plastics PA 12 TR Transparent Nylon 12 Used for optical components that benefit from the transparency and the high dynamic strengthProperties:TransparencyExtremely high dynamic strengthHigh chemical resistanceHigh stress-cracking resista.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | Conditioned; ISO 2039-1 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Ball Indentation Hardness | 90.0 MPa @Load 36.5 kg, Time 30.0 sec |
13100 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Ball Indentation Hardness | 90.0 MPa @Load 36.5 kg, Time 30.0 sec |
13100 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 757 G UV White 37019 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution PS 456EB HIPS Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | 358 N/30s; ISO 2039 |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H 385/30; ISO 2039 |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 3997 nat PAMACM12 Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H358/30; ISO 2039-1 |
Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H358/30; ISO 2039-1 |
Chi Mei Polylac® PA-758 ABS - Transparent Transparent |
|||
Ball Indentation Hardness | 90.0 - 145 MPa | 13100 - 21000 psi | ISO 2032-N961 |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 CI4 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic.. |
|||
Ball Indentation Hardness | 90.0 - 190 MPa | 13100 - 27600 psi | Average value: 144 MPa Grade Count:4 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLEN PP TV Polypropylene + talc This material is a low density, easily machined plastic that has good damping properties and is reinforced with talc for high rigidity. Applications include components for the electrical industry, h.. |