| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
| Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
| Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527-1,-2 |
| Elongation at Break | >= 15 % | >= 15 % | 50 mm/min; acc. ISO 527-1,-2 |
| Tensile Modulus | 2.05 GPa | 297 ksi | 1 mm/min; ISO 527-1,-2 |
| Flexural Strength | 62.0 MPa | 8990 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1A |
| 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A | |
| Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
| 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2; Parallel to Flow |
| CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75-1,-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 94.0 °C | 201 °F | ISO 75-1,-2 |
| Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
| 98.0 °C @Load 5.10 kg |
208 °F @Load 11.2 lb |
120°C/hour; ISO 306 | |
| Flame Spread | 63 mm/min | 2.5 in/min | (US-FMVSS); ISO 3795 |
| Glow Wire Test | 700 °C | 1290 °F | GWFI; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | IEC 60093 |
| Dielectric Constant | 2.9 @Frequency 100 Hz |
2.9 @Frequency 100 Hz |
IEC 60250 |
| 2.9 @Frequency 1.00e+6 Hz |
2.9 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Dielectric Strength | 35.0 kV/mm @Thickness 1.00 mm |
889 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
| Dissipation Factor | 0.0073 @Frequency 100 Hz |
0.0073 @Frequency 100 Hz |
IEC 60250 |
| 0.0090 @Frequency 1.00e+6 Hz |
0.0090 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
| Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 294 |
| Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |