| Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced |
| Manufacturer | Adamas |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adamas Rixon U PEEK, Unreinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
| Water Absorption | 0.10 - 0.50 % | 0.10 - 0.50 % | Immersion 24 hrs; ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 - 68 | 62 - 68 | ASTM D2240 |
| Ball Indentation Hardness | 90.0 - 145 MPa | 13100 - 21000 psi | ISO 2032-N961 |
| Tensile Strength at Break | 80.0 - 150 MPa | 11600 - 21800 psi | ASTM D638 |
| Elongation at Break | 20 - 40 % | 20 - 40 % | ASTM D638 |
| Tensile Modulus | 2.20 - 3.50 GPa | 319 - 508 ksi | ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 343 °C | 649 °F | DSC |
| Maximum Service Temperature, Air | 300 °C | 572 °F | DSC |
| Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | ASTM D149 |