Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 50.0 MPa | 7250 psi | |
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri.. |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
Polykemi AB SCANLON A 5005B PA/ABS-Blend Information provided by Polykemi AB |
|||
Flexural Strength | 50.0 MPa | 7250 psi | |
Plastcom SLOVALEN PH 59 T 40 LW 031 PP, 40% mineral filling, laser label FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG.. |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790-95 |
Multibase Multi-ABS 802 Natural Extrusion Grade Data provided by Multibase. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10 LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 400 Cast Polyamide 6, Elastomer Modified, Dry Application: gear-wheels, chain-wheels, hydrocyclones, housings, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 50.0 MPa | 7250 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
Stratasys® PC-ABS PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | Bending Strength |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East) Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | Bending Strength |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
Teknor Apex Sinpolene TPP1010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | GB/9341 |
Zhejiang Juner JEPPA003 High Glossy PP Applications: High Glossy PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ISO 178 |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | cond; ISO 178 |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ISO 178 |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Flexural Strength | 50.0 - 100 MPa | 7250 - 14500 psi | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ISO 178 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M40CL Mica Reinforced Coupled |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
Polykemi AB POLYfill PPH DNH15025 GF10 Polypropylene Homopolymer, Flame Retardant, Halogen Free, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 50.0 MPa | 7250 psi | ASTM D790 |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |