Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Modulus of Elasticity | 4.00 - 5.50 GPa | 580 - 798 ksi | |
Flexural Strength | 50.0 - 100 MPa | 7250 - 14500 psi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Specific Heat Capacity | <= 0.200 J/g-°C | <= 0.0478 BTU/lb-°F | |
Maximum Service Temperature, Air | 150 °C | 302 °F |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Magnetic Coercive Force, Hc | 1100 Oe | 1100 Oe | |
2890 Oe | 2890 Oe | Intrinsic | |
Magnetic Remanence, Br | 1250 Gauss | 1250 Gauss | |
Magnetic Maximum Energy Product, BH | 0.30 MGOe | 0.30 MGOe | |
Curie Temperature | 450 °C | 842 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Reversible Temp Coef., Bd | -0.20 %/°C | |
Reversible Temp Coef., Hd | +0.27 %/°C | |
Temperature Coefficient, Br | -0.2 %/°C | (20-100°C) |
Temperature Coefficient, Hci | +0.3 %/°C | (20-100°C) |