Material Notes:
Application: gear-wheels, chain-wheels, hydrocyclones, housings, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO R 1183
Moisture Absorption at Equilibrium 2.3 %
2.3 %
DIN 53473
Mechanical Properties Metric English Comments
Ball Indentation Hardness <= 100 MPa
<= 14500 psi
Hc 30; ISO 2039; partially
Tensile Strength, Yield 45.0 - 60.0 MPa
6530 - 8700 psi
ISO-DIS 527
Tensile Modulus >= 1.30 GPa
>= 189 ksi
DIN 53457
Flexural Strength <= 50.0 MPa
<= 7250 psi
DIN 54352
Flexural Modulus <= 2.00 GPa
<= 290 ksi
DIN 53457
Izod Impact, Notched (ISO) >= 10.0 kJ/m²
>= 4.76 ft-lb/in²
ISO 180-1A
Izod Impact Resistance NB
NB
swinging hammer 0,1 DIN 51222; DIN 53453
Tear Strength Test >= 0.45
>= 0.45
ISO-DIS 527
Thermal Properties Metric English Comments
CTE, linear 100 - 150 µm/m-°C

@Temperature 20.0 - 100 °C
55.6 - 83.3 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Melting Point 210 - 218 °C
410 - 424 °F
ISO R 1218
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
Deflection Temperature at 0.46 MPa (66 psi) 180 - 195 °C
356 - 383 °F
V-notch; ISO R 75
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Continuous