Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.0 - 85.0 MPa | 10900 - 12300 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
Nilit FRIANYL A63 E Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | <= 75.0 MPa | <= 10900 psi | ISO 178 |
Polykemi AB POLYabs F00 ABS Information provided by Polykemi AB |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
Nilit FRIANYL A63 HH Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat and hydrolysis stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
Nilit FRIANYL A63 KG20 Nylon 6.6 for injection molding, 20% chalk filled Nylon 6.6 for injection molding (low warpage and good form stability).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 2mm/min; ASTM D790 |
Kingfa MAC-601 UV PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® ABS 240 Injection Molding Grade Lustran® ABS 240 has standard impact strength and is injection molding grade. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Flexural Strength | 75.0 MPa @Strain 5.50 % |
10900 psi @Strain 5.50 % |
2 mm/min; ISO 178-A |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific) LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL004XXC Acetal Copolymer LNP LUBRICOMP* KL004XXC is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific) LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ISO 178 |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Flexural Strength | 75.0 MPa | 10900 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® GL6000 ABS Metal Plating Grade Excellent plating performance, Good thermal stabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | 75.0 - 110 MPa | 10900 - 16000 psi | ASTM D790-03 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |