Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nima™ NH PC151 Polycarbonate Non-Hal FR-PC with High HDT, high impact and improved processability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accordi.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Kolon KOCETAL® K300HRD Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific) LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM Test |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Flexural Strength | 77.0 MPa @Thickness 3.17 mm |
11200 psi @Thickness 0.125 in |
tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500 EF-Low Gel Extrusion Grade, Low Gel Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 77.0 MPa @Thickness 6.35 mm |
11200 psi @Thickness 0.250 in |
tangent; chs 2.5 in/min; 100 mm SL; ASTM D790 |
Diamond Polymers ABSPC 7330-1801H ABS/PC Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Resinoid 1329 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Strength | 77.0 MPa | 11200 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |