Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 195 MPa | 28300 psi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers.. |
|||
Flexural Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl LSE - OP66GF3015 Nylon 66 Low surface energy Nylon 66 for demanding applications such as bearings, bushes, rods and gearsAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Flexural Strength | <= 195 MPa | <= 28300 psi | ISO 178 |
Polykemi AB SCANAMID 66 A12^ F15 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 195 MPa | <= 28300 psi | ISO 178 |
Polykemi AB SCANAMID 66 A13^ F15 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S.. |
|||
Flexural Strength | 195 MPa | 28300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S.. |
|||
Flexural Strength | 195 MPa | 28300 psi | 2mm/min; ISO 178 |
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Flexural Strength | 195 MPa | 28300 psi | 2.8% strain; ISO 178 |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM-D790 |
Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber 20% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178-93 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM-D790 |
Polyram RamLloy PA917G6 PP/NYLON 66 alloy, 30% Glass Fiber 30% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced 30% Glass fiber reinforced Nylon6/PP alloy with reduced water absorption, dimensional stability and UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber 40% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 195 MPa | 28300 psi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO Data |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Strength | 195 MPa | 28300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
Flexural Strength | 195 MPa | 28300 psi | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |