Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Filler Content 10 %
10 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Tensile Strength 117 MPa
17000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
Flexural Strain; ASTM D790
4.9 %
4.9 %
ASTM D638
Tensile Modulus 3.45 GPa
500 ksi
ASTM D638
Flexural Strength 195 MPa
28300 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Compressive Strength 172 MPa
25000 psi
10% Deformation; ASTM D695
Compressive Modulus 3.10 GPa
450 ksi
ASTM D695
Izod Impact, Notched 0.294 J/cm
0.550 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved