| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Polypropylene (PP) |
| Manufacturer | Polyram |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.2 % | 1.2 % | 50% RH; ISO 62 |
| Water Absorption at Saturation | 3.0 % | 3.0 % | ISO 62 |
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 145 MPa | 21000 psi | ISO 527 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527 |
| Tensile Modulus | 5.90 GPa | 856 ksi | ISO 527 |
| Flexural Strength | 195 MPa | 28300 psi | ISO 178 |
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 218 °C | 424 °F | ISO 11357 |
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous use |
| 200 °C | 392 °F | Short peaks operation | |
| Flammability, UL94 | HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |