Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
double-gated; SABIC Method |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -20.0 °C |
2.06 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature -29.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature -20.2 °F |
ASTM D256 |
Styron Pulse® B-270 PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 2.1%); ASTM-D256 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp Applications:OphthalmicsOptical safety framesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, cla.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 285A3R30018 Butyrate Natural, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistanceInformation provided by Cossa Po.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 0.000 °C |
2.06 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1515 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood melt flow rate, good impact resistance, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -20.0 °C |
2.06 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 05100 GFC Polypropylene, 50% Glass Filled PP homopolymer 50% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0560 HFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedGood stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 0.000 °C |
2.06 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0580 GFC Polypropylene, 40% Glass Filled PP homopolymer 40% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |