Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.87 J/cm @Temperature -30.0 °C |
11.0 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -50.0 °C |
11.0 ft-lb/in @Temperature -58.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -17.8 °C |
11.0 ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® IP300 PC Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America.. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000H PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 12.7 mm |
11.0 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 786 ABS, Extrusion Grade Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac.. |
|||
Izod Impact, Notched | >= 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Izod Impact, Notched | >= 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6610A Impact Copolymer Polypropylene Impact Copolymer for Compounding and Injection Molded Applications Formolene® 6610A is a high impact copolymer of polypropylene designed for such injection applications as automotive compounding, l.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene Copolymer for Injection Molded Applications Requiring a Combination of High Toughness and Stiffness Formolene® 6613N is a copolymer of polypropylene designed and formulated for injection molding ap.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Dow 500.00 Developmental Performance Polypropylene Polymer D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applica.. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9420 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies .. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.20 mm |
11.0 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.20 mm |
11.0 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |